首页> 外文OA文献 >Preparation and photochromic properties of dye-doped aluminosilicate ORMOCER gels and coatings
【2h】

Preparation and photochromic properties of dye-doped aluminosilicate ORMOCER gels and coatings

机译:染料掺杂硅铝酸盐ORMOCER凝胶和涂料的制备及其光致变色性能

摘要

Aluminosilicate and ORMOCER gels and coatings containing photochromic dyes, 1, 3-dihydro-1, 3, 3-trimethylspiro-[2H-indole-2, 3u27-[3H]-naphth-[2, 1-b][1, 4]-oxazine] (SO) and 1u27, 8au27-dihydro-2u27, 3u27-dimethoxycarbonyl-spiro [fluorene-9, 1u27-indolizine] (DHI), were prepared by the sol-gel method and the photochromic activity was monitored in the course of the sol-wetgel-xerogel transformation. The photochromic activity of the aluminosilicate gels decreases rapidly and even vanishes in the wetgel-xerogel stage while that of ORMOCER gels and coatings levels off in the early wetgel-xerogel stage at a reasonably high photochromic intensity with the colour-fading speed similar to that in ethanol and the photostability being considerably improved. The experimental results are discussed in terms of the matrix effect on photochromism of organic dyes.
机译:含光致变色染料,1、3-二氢-1、3、3-三甲基螺-[2H-吲哚-2、3 u27- [3H]-萘-[2、1-b] [1]的硅铝酸盐和ORMOCER凝胶和涂料,4]-恶嗪](SO)和1 u27,8a u27-二氢-2 u27,3 u27-二甲氧基羰基-螺环[芴9,1 u27-吲哚利嗪](DHI)制备在溶胶-湿凝胶-干凝胶转化过程中监测溶胶-凝胶法和光致变色活性。铝硅酸盐凝胶的光致变色活性在湿凝胶-干凝胶阶段迅速下降,甚至消失,而ORMOCER凝胶和涂层在湿凝胶-干凝胶早期阶段以相当高的光致变色强度趋于平稳,其褪色速度与在乙醇和光稳定性大大提高。根据基质对有机染料光致变色的影响讨论了实验结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号