Silk sericin (SS)/silk fibroin (SF) blend nanofibers have been produced by electrospinning in a binary SS/SF trifluoroacetic acid (TFA) solution system, which was prepared by mixing 20 wt.% SS TFA solution and 10 wt.% SF TFA solution to give different compositions. The diameters of the SS/SF nanofibers ranged from 33 to 837 nm, and they showed a round cross section. The surface of the SS/SF nanofibers was smooth, and the fibers possessed a bead-free structure. The average diameters of the SS/SF (75/25, 50/50, and 25/75) blend nanofibers were much thicker than that of SS and SF nanofibers. The SS/SF (100/0, 75/25, and 50/50) blend nanofibers were easily dissolved in water, while the SS/SF (25/75 and 0/100) blend nanofibers could not be completely dissolved in water. The SS/SF blend nanofibers could not be completely dissolved in methanol. The SS/SF blend nanofibers were characterized by Fourier transform infrared (FTIR) spectroscopy, differential scanning calorimetry, and differential thermal analysis. FTIR showed that the SS/SF blend nanofibers possessed a random coil conformation and ß-sheet structure.
机译:通过在二元SS / SF三氟乙酸(TFA)溶液系统中进行电纺丝,已生产出丝胶蛋白(SS)/丝素蛋白(SF)共混纳米纤维,该体系是通过混合20 wt。%SS TFA溶液和10 wt。%SF制备的用TFA溶液给出不同的组成。 SS / SF纳米纤维的直径范围为33至837 nm,并且显示出圆形横截面。 SS / SF纳米纤维的表面是光滑的,并且纤维具有无珠的结构。 SS / SF(75 / 25、50 / 50和25/75)共混纳米纤维的平均直径比SS和SF纳米纤维的平均直径大得多。 SS / SF(100 / 0、75 / 25和50/50)共混纳米纤维很容易溶于水,而SS / SF(25/75和0/100)共混纳米纤维不能完全溶于水。 SS / SF共混纳米纤维无法完全溶解在甲醇中。 SS / SF混合纳米纤维的特征在于傅立叶变换红外(FTIR)光谱,差示扫描量热法和差热分析。 FTIR显示SS / SF混合纳米纤维具有无规卷曲构象和ß片状结构。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号