首页> 外文OA文献 >SEM-EDS analysis of glass fibers corroded in physiological solutions by dynamic tests with variable flow rates.
【2h】

SEM-EDS analysis of glass fibers corroded in physiological solutions by dynamic tests with variable flow rates.

机译:通过可变流速的动态测试,对在生理溶液中腐蚀的玻璃纤维进行SEM-EDS分析。

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。
获取外文期刊封面目录资料

摘要

The dissolution of mineral fibers has been studied in simulated physiological fluids using a dynamic testing procedure. Fibers of different chemical composition and obtained by different processes with a mean diameter of about 1 micron, have been characterized with respect to their solubility under various test conditions of flow-rate. The surfaces were analyzed using scanning electron microscopy (SEM), energy dispersive spectrometry (EDS) and X-ray diffraction techniques. SEM examinations show the formation of various corrosion patterns: porous, gel-like outer layers; precipitation zones and even, in some cases, no modification of the surface aspect. EDS analyses performed on the fibers, on the fiber surface layers, or on the deposits show three types of chemical composition: areas enriched in Al, in Ca and P, or in Al, Ca, and P. These surface compositions can be found for the same type of fiber tested, depending on the flow rate of the solution. Surface changes depend strongly on the initial composition of the glass and on the test conditions, particularly the flow rate. It is of particular interest to characterize the remaining surfaces (if any) obtained at the end of the in vitro test run and to compare them with surface analysis of the recovered fibers from the in vivo tests to assess the validity of the in vitro tests.
机译:已经使用动态测试程序研究了在模拟生理流体中矿物纤维的溶解情况。关于在不同的流速测试条件下的溶解度,已经表征了具有不同化学组成并且通过不同方法获得的平均直径为约1微米的纤维。使用扫描电子显微镜(SEM),能量色散光谱(EDS)和X射线衍射技术分析表面。 SEM检查显示出各种腐蚀模式的形成:多孔的凝胶状外层;沉淀区,甚至在某些情况下,不会改变表面外观。对纤维,纤维表面层或沉积物进行的EDS分析显示三种化学成分:富含Al,Ca和P或Al,Ca和P的区域。这些表面成分可用于取决于溶液的流速,是否测试了相同类型的纤维。表面变化在很大程度上取决于玻璃的初始组成和测试条件,特别是流速。特别有趣的是表征在体外测试运行结束时获得的剩余表面(如果有),并将其与体内测试回收的纤维的表面分析进行比较,以评估体外测试的有效性。

著录项

  • 作者

    Lehuédé, P; de Meringo, A;

  • 作者单位
  • 年度 1994
  • 总页数
  • 原文格式 PDF
  • 正文语种 {"code":"en","name":"English","id":9}
  • 中图分类

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号