首页> 外文OA文献 >Influence of aluminium sheet surface modification on the self-piercing riveting process and the joint static lap shear strength
【2h】

Influence of aluminium sheet surface modification on the self-piercing riveting process and the joint static lap shear strength

机译:铝板表面改性对自冲铆工艺及接头静态搭接剪切强度的影响

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Self-piercing riveting (SPR) has been widely used in automotive as one of the major joining technologies for aluminium structures due to its advantages over some of the more traditional joining technologies. Research has shown that friction is a very important factor that influences both the riveting process and the joint strength for SPR, but these influences have not been fully understood. In this paper, AA5754 sheets with different surface textures, such as original with solid wax, hot water washed, sandpaper ground and grit blasted, were used to study the influence of friction on therivet inserting process, joint features and static lap shear strength. The results of joint features and rivet setting displacement-force curve showed that hot water wash and sandpaper grinding on aluminium sheet did not have significant influence on the rivet inserting process and joint features; however, for joints with grit-blasted substrates, the rivet -setting forces were higher at the beginning, and a middle section of the curve and the joint features, such as interlocks and minimum remaining bottom material thickness (Tmin), were clearly altered. The lap shear tests showed that hot water washing can slightly increase the lap shear strength, sandpaper grinding increased the static lap shear strength further and grit blasting increased the static lap shear strength the most.
机译:自穿孔铆接(SPR)由于比其他一些传统的连接技术更具优势,因此已广泛用于汽车中,作为铝结构的主要连接技术之一。研究表明,摩擦是影响铆接过程和SPR接头强度的非常重要的因素,但这些影响尚未得到充分理解。本文采用不同表面纹理的AA5754板材,例如带有固体蜡的原件,热水洗涤,砂纸磨削和喷砂处理,研究了摩擦对铆钉插入过程,接缝特征和静态搭接剪切强度的影响。接头特征和铆钉设置位移力曲线的结果表明,铝板上的热水洗涤和砂纸磨削对铆钉的插入过程和接头特征没有显着影响。但是,对于带有喷砂基材的接头,铆钉固定力在开始时较高,并且曲线的中间部分和接头特征(例如互锁和最小剩余底部材料厚度(Tmin))明显改变。搭接剪切试验表明,热水洗涤可以略微提高搭接剪切强度,砂纸磨削进一步提高了静态搭接剪切强度,喷砂处理使静态搭接剪切强度最大。

著录项

  • 作者

    Li Dezhi;

  • 作者单位
  • 年度 2017
  • 总页数
  • 原文格式 PDF
  • 正文语种 en
  • 中图分类
  • 入库时间 2022-08-31 15:21:42

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号