首页> 外文OA文献 >Natural rubber latex used as drug delivery system in guided bone regeneration (GBR)
【2h】

Natural rubber latex used as drug delivery system in guided bone regeneration (GBR)

机译:天然橡胶胶乳在导向骨再生(GBR)中用作药物输送系统

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

In this work, we propose natural rubber latex (NRL) membranes as a protein delivery system. For this purpose Bovine Serum Albumin (BSA) was incorporated into the latex solution for in vitro protein delivery experiments. Different polymerization temperatures were used, from -10 to 27 °C, in order to control the membrane morphology. These membranes were characterized by Scanning Electron Microscopy (SEM), Atomic Force Microscopy (AFM), as well as the Lowry Method to measure the BSA release. SEM and AFM microscopy analysis showed that the number, size and distribution of pores in NRL membranes can be varied, as well as its overall morphology. We have found that the morphology of the membrane is the predominant factor for higher protein release, compared with pore size and number of pores. Results demonstrated that the best drug-delivery system was the membrane polymerized at RT (27 °C), which does release 66% of its BSA content for up to 18 days. Our results indicate that NRLb could be used in the future as an active membrane that could accelerate bone healing in GBR.
机译:在这项工作中,我们建议使用天然橡胶乳胶(NRL)膜作为蛋白质输送系统。为此目的,将牛血清白蛋白(BSA)掺入乳胶溶液中以进行体外蛋白质递送实验。为了控制膜的形态,使用了从-10到27℃的不同聚合温度。这些膜的特征在于扫描电子显微镜(SEM),原子力显微镜(AFM)以及用于测量BSA释放量的Lowry方法。 SEM和AFM显微镜分析表明,NRL膜中孔的数量,大小和分布以及其整体形态可以改变。我们已经发现,与孔径和孔数相比,膜的形态是较高蛋白质释放的主要因素。结果表明,最佳的药物递送系统是在室温(27°C)下聚合的膜,该膜在长达18天的时间内确实释放了其BSA含量的66%。我们的结果表明,NRLb将来可作为一种活性膜使用,可以加速GBR中的骨愈合。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号