This paper presents the evaluation of compressive strength of soil-cement bricks obtained by the inclusion in their mixture of PET flakes through mineral water bottles grinding. The Polyethylene Terephthalate (PET) has been characterized by its difficulty of disaggregation in nature, requiring a long period for this. On the other hand, with the increase in civil construction activities the demand for raw material also increases, causing considerable environmental impacts. In this context, the objective of this research is to propose a simple methodology, preventing its dumping and accumulation in irregular areas, and reducing the demand of raw materials by the civil construction industry. The results showed that compressive strengths obtained were lower than recommended by NBR 8491 (Associação Brasileira de Normas Técnicas [ABNT], 2012b) at seven days of curing time. However, they may be used as an alternative solution in masonry works in order to not submit themselves to great loads or structural functions. The studied bricks also presented water absorption near to recommended values by NBR 8491 (ABNT, 2012b). Manufacturing costs were also determined for this brick, comparing it with the costs of other brick types. Each brick withdrew from circulation approximately 300 g of PET waste. Thus, for an area of 1 m2 the studied bricks can promote the withdrawal of approximately 180 beverage bottles of 2 L capacity. 
机译:本文介绍了通过矿泉水瓶研磨将PET薄片混合物掺入水泥土砖获得的抗压强度。聚对苯二甲酸乙二酯(PET)的特征在于其本质上难以分解,为此需要很长时间。另一方面,随着民用建筑活动的增加,对原材料的需求也增加了,对环境造成了相当大的影响。在这种情况下,本研究的目的是提出一种简单的方法,防止其在不规则区域倾倒和堆积,并减少民用建筑业对原材料的需求。结果表明,在固化时间7天时,获得的抗压强度低于NBR 8491的推荐强度(AssociaçãoBrasileira de NormasTécnicas[ABNT],2012b)。但是,它们可以用作砌体工程的替代解决方案,以免使其承受巨大的荷载或结构功能。所研究的砖块的吸水率也接近NBR 8491(ABNT,2012b)的推荐值。还确定了该砖的制造成本,并将其与其他砖类型的成本进行比较。每块砖从循环中撤出了大约300克PET废料。因此,对于1平方米的区域,所研究的砖块可以促进大约2升容量的180个饮料瓶的抽出。