摘要

This study investigated the dimensional stability of denture bases influenced by packing methods, in relation to post-pressing times, in the Clássico acrylic resin which was prepared according to manufacturer recommendations. Forty maxillary wax bases were made and randomly assigned into 2 groups of 20 specimens each according to the conventional and RS system packing methods. In each method, the specimens were subdivided into immediate, 6, 12 and 24 h post-pressing times. The dough of the acrylic resin was packed in metallic flasks and processed in a water bath curing cycle at 74ºC for 9 h. After cooling at room temperature, the bases were removed from the flasks, finished and fixed on stone casts with instantaneous adhesive. The resin base-stone cast sets were transversally sectioned into 3 sections and the base-stone gap measured at 5 points in each section. The data were submitted to ANOVA and Tukey's test, which showed that the RS system had a smaller base distortion compared to conventional packing, with the exception of the 24-h post-pressing time. There was a statistically significant difference between the packing methods only in section C (posterior palatal zone). In the conventional packing method, the immediate and 6 h times demonstrated values with no statistically significant difference between them, as well as between the 12 and 24 h post-pressing times.
机译:这项研究调查了根据制造商的建议制备的Clásico丙烯酸树脂中受填充方法影响的义齿基托的尺寸稳定性与压后时间的关系。根据常规方法和RS系统包装方法,制作了40个上颌蜡基质,并随机分为两组,每组20个样品。在每种方法中,将样品分为紧压后的立即时间,6小时,12小时和24小时。将丙烯酸树脂的面团装入金属烧瓶中,并在74℃的水浴固化循环中处理9小时。在室温下冷却后,将基料从烧瓶中移出,整理并用瞬时粘合剂固定在石模上。将树脂基石铸件横向切成三段,并在每段中的五个点处测量基石间隙。数据已提交给ANOVA和Tukey检验,结果表明RS系统与常规包装相比具有更小的基础变形,除了24小时的压后时间。仅在C节(pa后区)之间的包装方法有统计学上的显着差异。在传统的包装方法中,即时和6小时显示的值在它们之间以及压制后12和24小时之间没有统计学上的显着差异。