Effect of non-solvent additives on the morphology and separation performance of poly(m-phenylene isophthalamide) (PMIA) hollow fiber nanofiltration membrane

机译:非溶剂添加剂对聚间亚苯基间苯二甲酰胺(PMIA)中空纤维纳滤膜形态和分离性能的影响

摘要

Newly designed poly(m-phenylene isophthalamide) (PMIA) hollow fiber nanofiltration membranes were fabricated containing non-solvent additives, i.e., lithium chloride (LiCl), acetone and PVP by dry-jet wet spinning technology. The effects of non-solvent additives on the morphology and separation performance were investigated. The addition of non-solvent additives in the dopes enhanced the viscosity significantly. The membrane cross-sections were monitored by scanning electron microscopy (SEM). The results indicated that by increasing the concentration of non-solvent additives, the morphologies changed from finger-like to sponge-like, and the outer skin-layer thickness was slightly increased. The rejections to various salts and pure water permeability (PWP) of these membranes were determined. The mean pore size and molecular weight cut-off (MWCO) were estimated using the solute rejection method. The results showed that the salt rejection of the membranes decreased in the order of R(Na2SO4) >R(MgSO4) >R(NaCl) >R(MgCl2), and as the concentrations of non-solvent additives increased, the PWPs, mean pore sizes and MWCOs of the PMIA membranes all decreased. The atomic force microscope (AFM) experiments demonstrated that a smooth membrane surface was formed by adding non-solvent additives. Furthermore, the stress values at break, the elongation at break and the elastic modulus of the fibers increased as non-solvent additive contents increased. (C) 2015 Elsevier B.V. All rights reserved.
机译:通过干喷湿法纺丝技术制备了含有非溶剂添加剂的新型设计的聚(间亚苯基间苯二甲酰胺)(PMIA)中空纤维纳滤膜,即氯化锂(LiCl),丙酮和PVP。研究了非溶剂添加剂对形态和分离性能的影响。在涂料中添加非溶剂添加剂可显着提高粘度。通过扫描电子显微镜(SEM)监测膜的横截面。结果表明,通过增加非溶剂添加剂的浓度,其形态从手指状变为海绵状,并且外皮层厚度略有增加。确定了这些膜对各种盐的排斥率和纯水渗透率(PWP)。平均孔径和截留分子量(MWCO)使用溶质排斥法估算。结果表明,膜的脱盐率按R(Na2SO4)> R(MgSO4)> R(NaCl)> R(MgCl2)的顺序降低,并且随着非溶剂添加剂浓度的增加,PWPs,平均值PMIA膜的孔径和MWCO均降低。原子力显微镜(AFM)实验表明,通过添加非溶剂添加剂可形成光滑的膜表面。此外,随着非溶剂添加剂含量的增加,纤维的断裂应力值,断裂伸长率和弹性模量增加。 (C)2015 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号