This paper introduces a new and effective method for preparation of PACl-electrolysis process. A series of PACl with high content of Al-13 polymer was successfully prepared by electrolysis process. The amount of Al-13 polymer formed in electrolysis process was found to be highly influenced by current density (d(i)), the distance between the electrodes, electrolysis time and the stirring rate of the electrolyte. For the Al-T (total aluminum concentration) of 2.0 M PACl obtained by electrolysis process, the optimal di and distance between the electrodes were 1.1 A dm(-2) and 10 mm respectively. The optimum circulating rate was 5.5 lh(-1). Because of the inhomogeneous pH between the surface of cathode and the bulk solution, the electrolysis process has the advantage to form more AI(OH)4 as precursor of Al-13 polymer. At the optimum condition, Al-13 polymer accounted for above 70% Of Al-T (PACl of Al-T = 2.0 M and B = 2.0), which was much higher than that of PACl prepared by other method. (C) 2003 Elsevier Ltd. All rights reserved.
机译:本文介绍了一种制备PACl电解工艺的有效方法。通过电解工艺成功制备了一系列高含量的Al-13聚合物的PACl。发现在电解过程中形成的Al-13聚合物的量受电流密度(d(i)),电极之间的距离,电解时间和电解质的搅拌速率的很大影响。对于通过电解工艺获得的2.0 M PACl的Al-T(总铝浓度),电极之间的最佳di和距离分别为1.1 A dm(-2)和10 mm。最佳循环速率为5.5 lh(-1)。由于阴极表面和本体溶液之间的pH值不均匀,因此电解过程具有形成更多的Al(OH)4作为Al-13聚合物前体的优势。在最佳条件下,Al-13聚合物占Al-T的70%以上(Al-T的PACl = 2.0 M,B = 2.0),远高于其他方法制备的PACl。 (C)2003 Elsevier Ltd.保留所有权利。

著录项

  • 作者

    Qu JH; Liu HJ;

  • 作者单位
  • 年度 2004
  • 总页数
  • 原文格式 PDF
  • 正文语种
  • 中图分类

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号