Plasma-sprayed mullite (3Al2O3 central dot 2SiO2) and mullite/yttria-stabilized-zirconia (YSZ) dual layer coatings have been developed to protect silicon-based ceramics from environmental attack. Mullite-based coating systems show excellent durability in air. However, in combustion environments, corrosive species such as molten salt or water vapor penetrate through cracks in the coating and attack the Si-based ceramics along the interface, Thus modification of the coating system for enhanced crack-resistance is necessary for long-term durability in combustion environments. Other key durability issues include interfacial contamination and coating/substrate bonding. Interfacial contamination leads to enhanced oxidation and interfacial pore formation, while weak coating/substrate bonding leads to rapid attack of the interface by corrosive species, both of which can cause premature failure of the coating. Interfacial contamination can be minimized by limiting impurities in coating and substrate materials. The interface may be modified to improve the coating/substrate bond.
机译:已经开发出等离子喷涂的莫来石(3Al2O3中心点2SiO2)和莫来石/氧化钇稳定的氧化锆(YSZ)双层涂层,以保护硅基陶瓷免受环境侵害。莫来石基涂料体系在空气中显示出出色的耐久性。但是,在燃烧环境中,诸如熔盐或水蒸气之类的腐蚀性物质会穿透涂层中的裂纹,并沿界面腐蚀Si基陶瓷。因此,为了长期的耐用性,有必要对涂层系统进行改进以提高其抗裂性在燃烧环境中。其他关键的耐用性问题包括界面污染和涂层/基材粘合。界面污染导致增强的氧化作用和界面孔的形成,而薄弱的涂层/底材结合力则导致腐蚀物质对界面的快速侵蚀,这两者都会导致涂层过早失效。通过限制涂料和基材中的杂质,可以最大程度地减少界面污染。可以修改界面以改善涂层/基底的结合。

著录项

  • 作者

    Lee Kang N.;

  • 作者单位
  • 年度 1999
  • 总页数
  • 原文格式 PDF
  • 正文语种
  • 中图分类

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号