An investigation of silicone elastomers for seals used in docking and habitat systems for future space exploration vehicles is being conducted at NASA. For certain missions, NASA is considering androgynous docking systems where two vehicles each having a seal would be required to: dock for a period of time, seal effectively, and then separate with minimum push-off forces for undocking. Silicone materials are generally chosen for their wide operating temperatures and low leakage rates. However silicone materials are often sticky and usually exhibit considerable adhesion when mated against metals and silicone surfaces. This paper investigates the adhesion unit pressure for a space rated silicone material (S0383-70) for either seal-on-seal (SoS) or seal-on-aluminum (SoAl) operation modes in the following conditions: as-received, after ground-based atomic-oxygen (AO) pre-treatment, after application of a thin coating of a space-qualified grease (Braycote 601EF), and after a combination of AO pre-treatment and grease coating. In order of descending adhesion reduction, the AO treatment reduced seal adhesion the most, followed by the AO plus grease pre-treatment, followed by the grease treatment. The effects of various treatments on silicone (S0383-70 and ELA-SA-401) outgassing properties were also investigated. The leading adhesion AO pretreatment reduction led to a slight decrease in outgassing for the S0383-70 material and virtually no change in ELA-SA-401 outgassing.
机译:NASA正在对用于未来太空探索飞行器的对接和栖息系统中的密封件使用的硅酮弹性体进行研究。对于某些任务,美国宇航局正在考虑采用雌雄同体的对接系统,其中要求两辆均带有密封件的车辆:对接一段时间,有效密封,然后以最小推力分离以进行对接。通常选择有机硅材料是因为它们具有宽的工作温度和低泄漏率。然而,硅酮材料通常是粘性的,并且当与金属和硅酮表面配合时通常表现出相当大的粘附性。本文研究了在以下条件下密封密封(SoS)或铝密封(SoAl)操作模式下,空间额定的有机硅材料(S0383-70)的粘合单元压力:接收后,研磨后基原子氧(AO)预处理,在施加空间合格的润滑脂(Braycote 601EF)的薄涂层后,以及AO预处理和润滑脂涂层的组合后。为了降低附着力,按照先后顺序进行AO处理可最大程度地降低密封件的附着力,然后进行AO加油脂预处理,然后再进行油脂处理。还研究了各种处理对有机硅(S0383-70和ELA-SA-401)除气性能的影响。领先的粘合AO预处理减少导致S0383-70材料的除气量略有减少,而ELA-SA-401除气率几乎没有变化。