Suitability of mixtures based on ethylene glycol and choline chloride is evaluated for the electrodeposition of magnetic SmCo alloys. Deep eutectic solvents (DES) are characterized by a wide electrochemical window, allowing the electrodeposition of metallic elements having a highly negative reduction potential. Electrodeposition of unconventional metals with reduction potential well below hydrogen evolution one is, in principle, feasible (e.g. Sm). Moreover, the limited presence of water during the growth of SmCo alloys may reduce oxidation and consequently improve the magnetic properties with respect to the employment of an aqueous bath. Deposits composition is strongly affected by process parameters and bath composition. Increasing choline chloride concentration and/or adding glycine to the solution allows to achieve higher Sm content in the deposit. Potentiostatic electrodeposition has been carried out in a conventional three electrodes cell, with potential interval selected from âu88u920.7 V vs Ag wire to âu88u920.95 V vs Ag wire, keeping the bath under stirring at 70°C. Magnetic SmCo films with composition from 0 to 50 wt% Sm have been obtained with coercivity up to 270 Oe.
机译:针对磁性SmCo合金的电沉积,评估了基于乙二醇和氯化胆碱的混合物的适用性。深共熔溶剂(DES)的特征在于宽的电化学窗口,可以电沉积具有高负还原电位的金属元素。还原电位远低于氢放出的非常规金属的电沉积原理上是可行的(例如Sm)。而且,在SmCo合金的生长过程中水的有限存在可以减少氧化,并因此改善关于使用水浴的磁性能。沉积物组成受工艺参数和熔池组成的强烈影响。增加氯化胆碱的浓度和/或向溶液中添加甘氨酸可实现沉积物中更高的Sm含量。恒电位电沉积已在常规的三电极电池中进行,电势间隔从“ Ag线”选择为“ to”到“ Ag线”为“ 920920.95 V”,保持浴液在70°C下搅拌C。已经获得具有0至50重量%Sm的组成的磁性SmCo膜,其矫顽力高达270Oe。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号