摘要

Versch. in: Journal of Oral Rehabilitation 2003 30; 265–269 Ceramic-fused-to-metal restorations are widely used in dentistry with a high degree of general success. Fracture of the ceramic eneers as a result of oral function or trauma is not an uncommon problem in clinical practice. Although fractures of such restorations do not necessarily mean the failure of the restoration, the renewal process is both costly and time consuming and therefore remains a clinical problem. Fractures in the anterior region pose an aesthetic problem but when they are in the posterior, chewing function could also be affected. The published literature reveals that reasons for failures cover a wide spectrum from iatrogenic factors to laboratory mistakes or because of factors related to the inherent structure of the ceramics or simply to trauma.
机译:Versch。见:《口腔修复杂志》 2003年30期; 265–269陶瓷熔融金属修复体在牙科领域得到广泛应用,取得了普遍成功。由于口腔功能或创伤导致的陶瓷烯的断裂在临床实践中并非常见问题。尽管这种修复体的断裂不一定意味着修复体的失败,但是更新过程既昂贵又费时,因此仍然是临床问题。前部骨折引起美学问题,但是当它们位于后部时,咀嚼功能也会受到影响。公开的文献表明,从医源性因素到实验室失误,或者由于与陶瓷的固有结构有关或与创伤有关的因素,失败的原因范围很广。

著录项

  • 作者

    Özcan M.;

  • 作者单位
  • 年度 2003
  • 总页数
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号