Gold catalysts based on ceria, doped by various RE metals (La, Sm, Gd, Yb, Y) were studied. The influence of the preparation methods on structure, properties and catalytic activity in the WGS reaction was investigated. The catalysts' supports were prepared using two different methods: co-precipitation (CP) and mechanochemical activation (MA). The catalysts were tested in a wide temperature interval without and after reactivation. All samples were characterized using a combination of X-ray diffraction (XRD), high resolution transmission electron microscopy (HRTEM), Raman spectroscopy (RS) and X-ray photoelectron spectroscopy (XPS) and TPR. It was found that the catalytic activity of MA catalysts is higher than CP ones. The gold catalysts based on ceria doped by Yb and Sm exhibited the highest activity. After reactivation in air the MA samples almost kept the WGS activity same, while the CP catalysts increased it. The catalysts of a single- and double-phase structure are formed as a result of CP and MA preparation, respectively. There are no big differences in the gold particles size (2-3 nm) depending on dopants and on the preparation techniques. The RS spectra analysis indicates that most probably the oxygen vacancies are adjacent to Me3+ dopant and the ceria structure seems to be better ordered than in the case of alumina as a dopant. There is no distinct correlation between reducibility and WGS activity. The XPS analysis disclose positively charged gold particles in addition to metallic gold within a surface region of fresh samples and only metallic gold on the samples after catalytic processing. There is no simple correlation between the concentration of Ce3+ in the samples and their WGS activity. © 2009 Elsevier B.V. All rights reserved.
机译:研究了以铈土为基础的金催化剂,并掺杂了各种稀土金属(La,Sm,Gd,Yb,Y)。研究了制备方法对WGS反应中结构,性质和催化活性的影响。催化剂的载体采用两种不同的方法制备:共沉淀(CP)和机械化学活化(MA)。在没有活化和活化后的宽温度区间内测试催化剂。所有样品均通过X射线衍射(XRD),高分辨率透射电子显微镜(HRTEM),拉曼光谱(RS)以及X射线光电子能谱(XPS)和TPR的组合进行表征。发现MA催化剂的催化活性高于CP催化剂。基于Yb和Sm掺杂的二氧化铈的金催化剂表现出最高的活性。在空气中重新活化后,MA样品几乎保持了WGS活性不变,而CP催化剂却提高了活性。 CP和MA的制备分别形成了单相和双相结构的催化剂。根据掺杂剂和制备技术,金的粒径(2-3 nm)没有太大差异。 RS光谱分析表明,氧空位最可能与Me 3+掺杂剂相邻,并且二氧化铈结构似乎比氧化铝作为掺杂剂的情况更好。可还原性与WGS活性之间没有明显的相关性。 XPS分析揭示了新鲜样品表面区域中除了金属金之外还带正电的金颗粒,催化处理后仅样品中的金属金。样品中Ce3 +的浓度与其WGS活性之间没有简单的相关性。 ©2009 Elsevier B.V.保留所有权利。