BaTiO3 (BT) powders were synthesized by the hydrothermal method for fabricating lead-free barium titanate piezoelectric ceramics. The obtained powders were washed by distilled water and 0.01 N acetic acid solutions separately, and utilized to obtain piezoelectric ceramics by traditional sintering. BT ceramics with the highest piezoelectric properties (d33 value is over 190 pC/N) was obtained from the BT powder synthesized at 250ºC and washed by acetic acid solution. The influence of washing method and sintering temperature on the piezoelectric properties of BT ceramics were studied. The reasons were investigated by comparing the properties of BT powders and their compacts sintered at different temperature.
展开▼
机译:采用水热法合成了BaTiO3(BT)粉末,制备了无铅钛酸钡压电陶瓷。将获得的粉末分别用蒸馏水和0.01N乙酸溶液洗涤,并用于通过传统烧结获得压电陶瓷。从250℃下合成的BT粉末中,用乙酸溶液洗涤,可获得具有最高压电性能(d33值超过190 pC / N)的BT陶瓷。研究了洗涤方法和烧结温度对BT陶瓷压电性能的影响。通过比较BT粉及其在不同温度下烧结的压粉的性能,研究了原因。
展开▼