首页> 外文OA文献 >Crystallographic texture in pulsed laser deposited hydroxyapatite bioceramic coatings
【2h】

Crystallographic texture in pulsed laser deposited hydroxyapatite bioceramic coatings

机译:脉冲激光沉积羟基磷灰石生物陶瓷涂层的晶体织构

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

The orientation texture of pulsed laser deposited hydroxyapatite coatings was studied by X-ray diffraction techniques. Increasing the laser energy density of the KrF excimer laser used in the deposition process from 5 to 7 J/cm2 increases the tendency for the c-axes of the hydroxyapatite grains to be aligned perpendicular to the substrate. This preferred orientation is most pronounced when the incidence direction of the plume is normal to the substrate. Orientation texture of the hydroxyapatite grains in the coatings is associated with the highly directional and energetic nature of the ablation plume. Anisotropic stresses, transport of hydroxyl groups and dehydroxylation effects during deposition all seem to play important roles in the texture development.
机译:通过X射线衍射技术研究了脉冲激光沉积羟基磷灰石涂层的取向织构。将沉积过程中使用的KrF准分子激光器的激光能量密度从5 J / cm2增加到7 J / cm2,增加了羟基磷灰石晶粒的c轴垂直于基板排列的趋势。当羽流的入射方向垂直于基底时,该优选取向最明显。涂层中羟基磷灰石晶粒的取向织构与烧蚀羽流的高度定向性和高能性质有关。各向异性应力,羟基的运输和沉积过程中的脱羟基作用似乎都在质地发展中起重要作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号