The possibilities offered by the EIS technique for studying the progress of corrosion in several types of galvanised coatings were investigated. Corrosion tests were performed in a 3 wt.% NaCl aqueous solution, at approximately neutral pH, without stirring and in contact with the air. A tendency was seen towards an electrochemical overestimation of the corrosion values of essentially pure zinc and Zn-5%Al (Galfan) coatings compared with the gravimetric reference values. In contrast, the opposite tendence was revealed with the Zn-10%Fe (Galvanneal) coating. These deviations have made it necessary to use empirical values of the constant B of the Stern-Geary equation. The approximately linear progress of the attack with immersion time suggests a slight barrier effect of the corrosion products layer. © 2004 Elsevier Ltd. All rights reserved.
机译:EIS技术为研究几种类型的镀锌涂层中的腐蚀进程提供了可能性。腐蚀试验是在3%(重量)的NaCl水溶液中,在大约中性pH值下进行的,无需搅拌并且与空气接触。与重量参考值相比,人们看到了一种化学上高估基本纯锌和5%Al(Galfan)镀层腐蚀值的趋势。相反,Zn-10%Fe(镀铝锌)涂层显示出相反的趋势。这些偏差使得必须使用Stern-Geary方程常数B的经验值。腐蚀与浸入时间的线性关系表明腐蚀产物层有轻微的阻挡作用。 ©2004 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号