From coal-mining waste to construction material: a study of its mineral phases

机译:从采矿废料到建筑材料:矿物相研究

摘要

The study from the recycling of coal mining waste from NW of Spain as pozzolans materials in cement industry is the scope of this present study. The thermal activation of coal-mining wastes, the formation of their hydrated phases and their evolution are analyzed, over pozzolanic reactions at 1, 7 and 28 days following activation. The coal-mining waste showed good pozzolanic activity, following thermal activation at 600 and 900 °C for 2 h. Total destruction of kaolinite is produced after treatment at 600 °C/2 h retention in the oven. This temperature and time are best suited for activation of the best environmental way. The compounds arising during the pozzolanic reaction in coal-mining waste activated at 600° and 900° in a Ca(OH)2 system were C–S–H gels, stratlingite (C2ASH8), tetracalcium aluminate hydrate (C4AH13), layered double hydroxides and monosulfoaluminate. When the temperature is 600 °C appeared layered double hydroxides via the metastable phase is favored during the first 7 days of reaction, while stratlingite is present as the major crystalline phase at 28 days into the pozzolanic reaction.
机译:来自西班牙西北部的煤矿废料作为水泥工业中的火山灰材料的回收利用是本研究的范围。在活化后1、7和28天,通过火山灰反应分析了采煤废物的热活化,水合相的形成及其演变。在600和900°C下热活化2小时后,采煤废料表现出良好的火山灰活性。在烤箱中保持600°C / 2 h处理后,会完全破坏高岭石。此温度和时间最适合激活最佳环境方式。在Ca(OH)2系统中于600°和900°活化的煤矿废料中,火山灰反应过程中产生的化合物为C–S–H凝胶,钙钛矿(C2ASH8),铝酸四钙水合物(C4AH13),层状双氢氧化物和一水合硫酸铝。当温度为600°C时,在反应的前7天出现了通过亚稳相形成的层状双氢氧化物,而钙钛矿则在火山灰反应发生后的28天时作为主要的结晶相存在。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号