摘要

Two industrial coal blends (B1 and B2) used in cokemaking were selected for this study. Two wastes from scrap tyres (TC, F) were added to these coal blends at different ratios (98:2 and 95:5). The investigation was focused on assessing the influence of the additives on thermoplastic properties of coal by means of the Gieseler fluidity test and thermogravimetric analysis. In addition, the blends were carbonized in a 17 kg electrically heated movable wall oven in order to examine the quality of the resultant cokes. Quality of the cokes produced was evaluated by measuring their cold mechanical strength, reactivity and post-reaction strength. It was found that ash composition of the additives contribute to a deterioration in coke quality. Moreover, F causes a greater decrease in coke strength after reaction with CO2 due to the diminution of bulk density in the coking process and to the higher basicity index. Trace elements were also studied in relation to waste addition.
机译:本研究选择了两种用于炼焦的工业煤混合物(B1和B2)。将废轮胎的两种废料(TC,F)以不同的比例(98:2和95:5)添加到这些煤混合物中。该研究的重点是通过Gieseler流动性测试和热重分析评估添加剂对煤热塑性特性的影响。另外,将掺合物在17kg电加热的可移动壁式炉中碳化以检查所得焦炭的质量。通过测量其冷机械强度,反应性和反应后强度来评估所生产焦炭的质量。发现添加剂的灰分组成导致焦炭质量的劣化。而且,由于在焦化过程中堆积密度的降低和较高的碱度指数,F导致与CO 2反应后焦炭强度的更大降低。还研究了与废物添加有关的微量元素。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号