Corrosion rate and corrosion product characterisation using Raman spectroscopy for steel embedded in chloride polluted fly ash mortar

机译:用拉曼光谱法对嵌入氯化物污染的粉煤灰砂浆中的钢进行腐蚀速率和腐蚀产物表征

摘要

Electrochemical impedance spectroscopy (EIS) and polarisation curves assisted by Raman spectroscopy were used to study the corrosion behaviour and to characterise the corrosion products of reinforcing steel embedded in fly ash mortars with and without chloride pollution. Two alkaline solutions with different soluble silica contents were utilised to activate the fly ash. After 720 days of experimentation the reinforcing steel embedded in fly ash mortar without chlorides remained passive, while the specimens in fly ash polluted with chloride ions (0.4 and 2%) yielded current density values of the order of 2 × 10-5 A/cm2, typical of an active state. The main corrosion products identified on the steel surface were less crystallised phases of iron oxyhydroxide hydrates and goethite (α-FeOOH) or lepidocrocite (γ-FeOOH). © 2013 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
机译:利用电化学阻抗谱(EIS)和拉曼光谱辅助的极化曲线研究了腐蚀行为并表征了埋入粉煤灰砂浆中的钢筋在有无氯污染的情况下的腐蚀产物。利用具有不同可溶性二氧化硅含量的两种碱性溶液来活化飞灰。经过720天的实验,埋在粉煤灰砂浆中的无氯钢筋仍然保持被动状态,而粉煤灰中的标本被氯离子(0.4和2%)污染时,其电流密度值约为2×10-5 A / cm2 ,通常是活跃状态。在钢表面上发现的主要腐蚀产物是氢氧化铁水合物和针铁矿(α-FeO​​OH)或纤铁矿(γ-FeOOH)的结晶度较低的相。 ©2013 WILEY-VCH Verlag GmbH&Co. KGaA,Weinheim。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号