Vliv kalcinační teploty a doby kalcinace na kompozit kaolinit/TiO2 pro fotokatalytickou redukci CO2

机译:煅烧温度和煅烧时间对高岭土/ TiO2复合材料光催化还原CO2的影响

摘要

The kaolinite/TiO2 composite (60 wt% of TiO2) was prepared by thermal hydrolysis of a raw kaolin suspension in titanyl sulphate and calcined at different temperatures (600, 650 and 700°C) and for different times (1, 2 and 3 h). The obtained samples were characterized by XRPD, N2 physical adsorption and SEM, and tested for photocatalytic reduction of CO2. The different calcination conditions did not influence TiO2 phase composition, only slightly changed the specific surface area, and significantly affected crystallite size of kaolinite/TiO2 composite. A higher temperature and longer duration of calcination lead to higher crystallinity of the powder. The photocatalytic results showed that the crystallite size determined the efficiency of kaolinite/TiO2 photocatalysts.
机译:高岭石/ TiO2复合材料(TiO2的60 wt%)是通过将粗高岭土悬浮液在硫酸氧钛中热水解制备的,并在不同的温度(600、650和700°C)和不同的时间(1、2和3 h)下煅烧)。通过XRPD,N2物理吸附和SEM对所得样品进行表征,并测试了光催化还原CO2的能力。不同的煅烧条件不会影响TiO2相的组成,只会稍微改变比表面积,并显着影响高岭土/ TiO2复合物的微晶尺寸。较高的温度和较长的煅烧时间导致粉末的较高结晶度。光催化结果表明,微晶尺寸决定了高岭土/ TiO2光催化剂的效率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号