首页> 外文OA文献 >Tailored setting times with high compressive strengths in bassanite calcium sulfoaluminate eco-cements
【2h】

Tailored setting times with high compressive strengths in bassanite calcium sulfoaluminate eco-cements

机译:用高抗压强度定制的含有高抗压强度的含钙硫化钙钙质生态水泥

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

This work deals with the hydration of a calcium sulfoaluminate (CSA) eco-cement prepared with bassanite and different additives (type and content) at a fixed water/CSA ratio of 0.5. Pastes prepared with bassanite show high water demands, high viscosity values and short initial setting times which are related to the fast dissolution rate of bassanite and the subsequent precipitation of gypsum. These facts have a dramatic effect onto the mechanical strength values, and make necessary the addition of additives.Here, the addition of different amounts of specific retarders (polycarboxylate, tartaric acid and phosphonic acid) not only improved the workability of pastes and mortars, but also delayed the setting time, by modifying the dissolution rates of the phase(s), and improved mechanical strengths. Finally, mortars with high compressive strengths (46 and 84 MPa at 1 and 7 days of hydration, respectively) and, chiefly, tailored setting times with high strengths have been prepared.
机译:这项工作涉及以固定的水/ CSA比值为0.5的条件,用重钙铝石和不同的添加剂(类型和含量)制备的硫铝酸钙(CSA)生态水泥的水合作用。用重晶石制备的糊显示出高的需水量,高的粘度值和较短的初始凝固时间,这与重晶石的快速溶解速率和随后的石膏沉淀有关。这些事实对机械强度值产生了巨大影响,并需要添加添加剂。在这里,添加不同量的特定缓凝剂(聚羧酸盐,酒石酸和膦酸)不仅改善了糊剂和砂浆的可加工性,而且通过改变相的溶解速率,还可以延长凝固时间,并提高机械强度。最终,制备了具有高抗压强度(分别在水合1天和7天时分别为46和84 MPa),主要是定制的具有高强度的凝固时间的砂浆。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号