Effect of high-speed parameters on uncoated carbide tooludin finish turning titanium Ti-6Al-4V ELI

机译:高速参数对无涂层硬质合金刀具的影响 ud精加工钛Ti-6Al-4V ELI

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

In this work, the Sandvik uncoated carbide insert, CNGG 120408-SGF-H13A was used as a cutting tool in high-speed turning of titanium alloy Ti-6Al-4V ELI (extra-low interstitial) with hardness of 32 HRC. Wear is one of the problems that cannot be avoided in machining process. Therefore, the objective of this paper was to investigate tool-wear behavior of various cutting-speed values (high-speed range) on the tool life of the cutting tools, especially in finishing titanium alloy. The experiments were performed under flooded coolant condition using water-based mineral-oil. The cutting speeds employed were 120, 170 and 220 m/min. The feed rate was constant at 0.2 mm/rev and the depth of cut was 0.4 mm. Based on the results, the highest cutting speed of 220 m/min caused the highest wear rate. By linking the machine operations and the tool life curves obtained using flank wear data, the wear behavior of uncoated carbide was described.
机译:在这项工作中,山特维克无涂层硬质合金刀片CNGG 120408-​​SGF-H13A用作高速车削硬度为32 HRC的钛合金Ti-6Al-4V ELI(极低间隙)的切削工具。磨损是机加工过程中无法避免的问题之一。因此,本文的目的是研究各种切削速度值(高速范围)对刀具寿命,特别是在精加工钛合金中的刀具磨损行为。实验是在使用水基矿物油的冷却液驱油条件下进行的。所采用的切割速度为120、170和220 m / min。进给速度恒定为0.2 mm / rev,切削深度为0.4 mm。根据结果​​,最高切削速度为220 m / min导致最高磨损率。通过链接使用侧面磨损数据获得的机器操作和刀具寿命曲线,描述了未涂层硬质合金的磨损行为。