摘要

Neodymium:yttrium-aluminum-garnet (Nd:YAG) laser may cause intraocular lenses (IOLs) damages. Therefore, the effects of Nd:YAG laser on IOLs were evaluated. Twenty-four IOLs (copolymer of 2-hydroxyethylmethacrylate and 2-ethoxyethylmethacrylate) were used. For scanning electron microscope (SEM), twelve IOLs were divided into three groups: Group 1, controls; Group 2, IOLs treated with two laser spots (YC-1800 Nidek Nd:YAG laser set at 1.2 mJ); and Group 3, IOLs treated with six laser spots. All IOLs were critical point dried in CO2 and viewed in a Zeiss EVO LS10 SEM. For Energy Dispersive X-ray spectrometry (EDX), four IOLs of each group were examined with a Jeol JMC-6000 SEM. With SEM, Group 1 IOLs showed well-preserved size, shape and surface. Group 2 IOLs exhibited normal shape and margins, a peripheral furrow with irregular blebs, straight clefts and holes on the wrinkled surface. Group 3 IOLs were swollen and broken into two or three parts. With SEM and EDX, Group 1 and the undamaged surfaces of Groups 2 and 3 showed evident carbon and oxygen peaks, while, in the damaged areas, both atoms were significantly reduced. Nd:YAG laser induced evident changes in IOLs morphology and organic alterations in their chemistry: great care during posterior capsule opacification treatment is required.
机译:钕:钇 - 铝 - 石榴石(ND:YAG)激光器可能导致眼透镜(IOL)损坏。因此,评估了Nd:YAG激光对IOL的影响。使用二十四种IOL(2-羟乙基甲基丙烯酸甲酯和2-乙氧基乙基丙烯酸甲酯的共聚物)。对于扫描电子显微镜(SEM),将12个IOL分为三组:第1组,控制;第2组,用两个激光斑点处理的IOL(YC-1800 NDK ND:YAG激光设定为1.2 MJ);和第3组,IOL用六个激光斑点处理。所有IOL在CO2中的关键点是致力的,并在Zeiss Evo LS10 SEM中观看。对于能量分散X射线光谱法(EDX),用JEOL JMC-6000 SEM检查每组的四个IOL。使用SEM,第1组IOL显示出保存完好的尺寸,形状和表面。第2组IOL表现出正常的形状和边缘,一个外围沟槽,带有不规则的灼热,直线裂缝和皱纹表面上的孔。第3组IOL肿胀并分为两三个部分。对于SEM和EDX,组1和组2和3的未损坏表面显示了明显的碳​​和氧峰,而在受损区域中,两种原子都显着降低。 ND:YAG激光诱导的IOL形态和化学有机改变的变化:需要在后胶囊渗透处理过程中的优点。