A series of catalysts of Ag2O-Co3O4/γ-Al2O3 was prepared by equivalent volume impregnation method. The effects of the metal loading, calcination time, and calcination temperatures of Ag and Co, respectively, on the catalytic activity were investigated. The optimum preparing condition of Ag2O-Co3O4/γ-Al2O3 was decided, and then the influence of different preparation conditions on catalytic activity of Ag2O-Co3O4/γ-Al2O3 was analyzed. The results showed the following: (1) at the same preparation condition, when silver loading was 8%, the Ag2O-Co3O4/γ-Al2O3 showed higher catalyst activity, (2) the catalyst activity had obviously improved when the cobalt loading was 8%, while it was weaker at loadings 5% and 10%, (3) the catalyst activity was influenced by different calcination temperatures of silver, but the influences were not marked, (4) the catalyst activity can be influenced by calcination time of silver, (5) different calcination times of cobalt can also influence the catalyst activity of Ag2O-Co3O4/γ-Al2O3, and (6) the best preparation conditions of the Ag2O-Co3O4/γ-Al2O3 were silver loading of 8%, calcination temperature of silver of 450°C, and calcinations time of silver of 4 h, while at the same time the cobalt loading was 8%, the calcination temperature of cobalt was 450°C, and calcination time of cobalt was 4 h.
机译:通过当量的体积浸渍方法制备一系列Ag2O-Co3O4 /γ-Al 2 O 3催化剂。研究了Ag和Co的金属负载,煅烧时间和煅烧温度对催化活性的影响。确定了Ag 2 O-CO 3 O 4 /γ-Al 2 O 3的最佳制备条件,分析了不同制剂条件对Ag2O-CO 3 /γ-Al2O3催化活性的影响。结果表明:(1)在相同的制备条件下,当银载荷为8%时,Ag2O-Co3O4 /γ-Al 2 O 3显示出更高的催化剂活性,(2)当钴载荷为8时,催化剂活性明显改善%,虽然载荷较弱5%和10%,(3)催化剂活性受银的不同煅烧温度的影响,但不标记的影响,(4)催化剂活性可以受银煅烧时间的影响,(5)钴的不同煅烧时间也可以影响Ag 2 O-Co3O4 /γ-Al2O3的催化剂活性,(6)Ag2O-Co3O4 /γ-Al2O3的最佳制备条件是8%,煅烧温度的银载负荷450°C的银,和煅烧时间为4小时,虽然同时钴载荷为8%,煅烧温度为450℃,钴的煅烧时间为4小时。