In this study, natural clay minerals with green appearance were treated with sulfuric acid. Mass percentage of acid (wt%), temperature (T), contact time (t) and liquid-to-solid mass ratio (R) are used as the prevailing factors that determine the extent of acid-activation. The values of these factors range from 15⁻50%, 60⁻90 °C, 1.5⁻6 h and 4⁻7, respectively. The study has focused on the structural changes as well as textural characteristics of the clay. Three activated clay samples were prepared under different treatment conditions. The samples were characterized using X-ray powder diffraction (XRD), fourier transform infrared (FTIR), scanning electron microscope (SEM), chemical analysis and N2 adsorption techniques. Characterization of the treated clay minerals exhibited significant structural changes to a greater extent of acid-activation, from being partially crystalline to being amorphous silica. The surface area and total pore volume of clay increased proportionally with the level of acid treatment. The average pore diameter behaved differently. During the strong acid treatment, a large increase in pore volume and the enlargement of the pore size distribution were observed. This suggests that considerable structural changes and partial destruction may have occurred in this condition. The removal of methylene blue, used as cationic dye, from aqueous solution by the batch adsorption technique on three prepared acid-activated clay samples was studied. The Langmuir model was found to agree well with the experimental data.
机译:在这项研究中,用硫酸处理具有绿色外观的天然粘土矿物。用作确定酸活化程度的酸(WT%),温度(T),接触时间(T)和液态质量比(R)的质量百分比用作酸活化程度的普遍因素。这些因素的值分别为15±50%,60°C,1.5±6小时和4×7。该研究专注于结构性变化以及粘土的纹理特征。在不同的处理条件下制备三个活化的粘土样品。使用X射线粉末衍射(XRD),傅里叶变换红外(FTIR),扫描电子显微镜(SEM),化学分析和N 2吸附技术。经处理的粘土矿物的表征表现出显着的结构变化,以更大程度的酸活化,部分结晶为无定形二氧化硅。粘土的表面积和总孔体积与酸处理水平成比例地增加。平均孔径表现不同。在强酸处理期间,观察到孔隙体积大幅增加和孔径分布的扩大。这表明在这种情况下可能发生了相当大的结构变化和部分破坏。研究了通过批量吸附技术在三种制备的酸活化粘土样品中从水溶液中除去亚甲基蓝。发现Langmuir模型与实验数据很好。