首页> 外文OA文献 >An effective process for simultaneous extraction of valuable metals (V, Cr, Ti, Fe, Mn) from vanadium slag using acidic sodium chlorate solution under water bath conditions
【2h】

An effective process for simultaneous extraction of valuable metals (V, Cr, Ti, Fe, Mn) from vanadium slag using acidic sodium chlorate solution under water bath conditions

机译:在水浴条件下使用酸性氯酸钠溶液同时提取钒渣的有价值金属(V,Cr,Ti,Fe,Mn)的有效方法

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

In the present work, a novel process for effective extraction of valuable metals (V, Cr, Ti, Mn, Fe, Al, and Mg) from the vanadium slag is proposed. The leaching parameters for valuable metals extraction from the vanadium slag by acidic sodium chlorate solution were studied to obtain conditions for vanadium to be leached without using a pyro metallurgical step since the roasting process requires high energy consumption. The optimal H2SO4 concentration, weight ratio of NaClO3 to sample, leaching time, leaching temperature, agitation speed and ratio of liquid volume to solid mass were 6 M, 0.2, 6 h, 95℃, 200 rpm and 10, respectively. Under these optimal conditions, the extraction ratio of vanadium and valuable metals (V, Cr, Ti, Mn, Fe, Al, and Mg) were 85.8% and 91.2%, respectively. Compared with salt roasting, this process could simultaneously extract valuable metals from vanadium slag. More importantly, the experimental temperature was low underwater bath conditions.
机译:在本作研究中,提出了一种新的方法,用于有效提取来自钒渣的有效萃取有价值金属(V,Cr,Ti,Mn,Fe,Al和Mg)的过程。研究了来自钒渣的有价值金属的浸出参数,通过酸性氯酸钠溶液中萃取,得到钒钒的条件,而不使用PyRO冶金步骤,因为焙烧过程需要高能量消耗。最佳的H 2 SO 4浓度,NaClO3与样品的重量比,浸出时间,浸出温度,搅拌速度和液体体积与固物的比例分别为6米,0.2,6h,95℃,200rpm和10。在这些最佳条件下,钒和有价值金属(V,Cr,Ti,Mn,Fe,Al和Mg)的提取比分别为85.8%和91.2%。与盐焙烧相比,该方法可以同时从钒渣中提取有价值的金属。更重要的是,实验温度低水水浴条件。