Low-Temperature Tar Content of Bituminous Materials. Part 1. Dense Tar Surfacing with Crushed Rock Aggregate

机译:沥青材料的低温焦油含量。第1部分。密集焦油与碎石混合物堆焊

获取原文

摘要

The limited study using the two crushed rock aggregates with high- and low-density tars of coke-oven and low-temperature carbonization sources has shown that equal volumes of tar are required, regardless of carbonization source. It is recommended that, when the density of the tar is below 1.12 g/ml, an additional reduction in tar content of 0.3% by mass should be applied to the recommendations in the British Standard. (ERA citation 05:028327)