ELECTROCHEMICAL CORROSION TESTS FOR TANK 241-AY-101 CORE 325 SEGMENTS 16R1 & 16R2

机译:用于坦克241-aY-101核心325段16R1和16R2的电化学腐蚀试验

获取原文

摘要

The interstitial liquid in the double-shell tank 241-AY-101 settled solids layer is below the hydroxide chemistry control limit required by HNF-SD-WM-TSR-006, Tank Farms Technical Safety Requirements, Administrative Control 5.16, 'Corrosion Mitigation Controls'. Operating tanks outside of the specification may increase the propensity corrosion of the carbon steel wall. This report is concerned with generalized electrochemical corrosion mechanism that may occur at specific loci. All cyclic potentiodynamic polarization scans exhibited a negative hysteresis, scan reversing at lower current density, indicating that there was no pitting propensity. The general electrochemical corrosion rates ranged from 4.4E-02 to 1.5E-03 mpy with the first round of coupons, while the second round yielded corrosion rates of 2.5E-03 to 2.9E-02 mpy.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号