首页> 美国政府科技报告 >Investigation on the Use of a Laser Ablation Treatment on Metallic Surfaces and the Influence of Temperature on Fracture Toughness of Hybrid Co-Cured Metal-PMC Interfaces.
【24h】

Investigation on the Use of a Laser Ablation Treatment on Metallic Surfaces and the Influence of Temperature on Fracture Toughness of Hybrid Co-Cured Metal-PMC Interfaces.

机译:金属表面激光烧蚀处理及温度对混合共固化金属-pmC界面断裂韧性影响的研究。

获取原文

摘要

Hybrid composite laminates that contain alternating layers of titanium alloys and carbon fabric reinforced polyimide matrix composites (PMC) are excellent candidates for light-weight, high-temperature structural materials for high-speed aerospace vehicles. The delamination resistance of the hybrid titanium-PMC interface is of crucial consideration for structural integrity during service. Here, we report the first investigations on the use of laser ablation in combination with sol-gel treatment technique on Ti/NiTi foil surfaces in co-cured hybrid polyimide matrix composite laminates. Mode-I and mode-II fracture toughness of the hybrid Ti/NiTi-PMC interface as a function of temperature were determined via experimental testing and finite element analysis.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号