PREPARATION AND PROPERTIES OF CONSUMABLE-ELECTRODE VACUUM-ARC-MELTED ELECTROLYTIC IRON

机译:消耗电极真空电弧熔融电解铁的制备与性能

获取原文

摘要

Oxygen was removed from a relatively pure grade of electrolytic iron by a solid-state, hydrogen reduction treatment prior to vacuum arc melting. Consumable electrode arc melting into a water-cooled copper crucible excluded contamination. The initial oxygen content of 400 ppm was reduced to below 50 ppm in the ingot. The values of various physical (density, electrical resistivity, thermoelectric force, and magnetic) and mechanical (tensile strength, Charpy V notch, and hardness) properties were measured to assess the quality of this iron, which compares favorably with research grades described in the literature.

著录项

  • 作者

    R. W. Huber;

  • 作者单位
  • 年度 1963
  • 页码 1-18
  • 总页数 18
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类 工业技术;
  • 关键词

  • 入库时间 2022-08-29 11:43:50

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号