首页> 外文期刊>Solid state sciences >Synthesis and thermoelectric properties of Sr_0.95La0.05TiO_(3-delta)-TiO_2 solid solutions
【24h】

Synthesis and thermoelectric properties of Sr_0.95La0.05TiO_(3-delta)-TiO_2 solid solutions

机译:Sr_0.95La0.05TiO_(3-δ)-TiO_2固溶体的合成及热电性能

获取原文
获取原文并翻译 | 示例
           

摘要

Sr_0.95La0.05TiO_(3-delta) solid solutions, combined with 10 molpercent TiO_2, were prepared at different temperatures. When sintered at a suitable temperature, the Seebeck coefficient presents the same behavior at high temperatures as that of Sr0.95Lao.o5Ti03_a ceramic. Otherwise, the Seebeck coefficient would be smaller. After introducing TiO_2, both of the thermal and electrical conductivity are reduced. The sample sintered at 1350 degC exhibits the highest ZT of about 0.2, which slightly larger than that of Sr_0.95La0.05TiO_(3-delta) ceramic.
机译:在不同温度下制备了Sr_0.95La0.05TiO_(3-δ)固溶体和10 mol%TiO_2。当在适当的温度下烧结时,塞贝克系数在高温下表现出与Sr0.95Lao0.5TiO3_a陶瓷相同的行为。否则,塞贝克系数将更小。引入TiO_2后,导热率和导电率均降低。在1350℃下烧结的样品具有最高的ZT,约为0.2,比Sr_0.95La0.05TiO_(3-δ)陶瓷的ZT稍大。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号