CeO2-TiO2 thin films have been deposited onto glass substrates by spin coating method with 2500, 3000, and 4000 rpm spin rates using sol-gel process. The time effect on the optical properties of the films has been investigated by evaluating the variation of spectral behavior over a period of about 11 weeks. In the first week of aging, the optical indices of the films show observable variation. After four weeks, the changes reduce, and these parameters become constant approximately after six weeks. After 11 weeks of aging it was found that the refractive index of the CeO2-TiO2 thin films is 1.91 +/- 0.03, 1.98 +/- 0.04, and 1.10 +/- 0.02, and extinction coefficient is 2.8 +/- 0.2 x 10(-3), 3.3 +/- 0.2 x 10(-3) and 3.8 +/- 0.3 x 10(-3) for spinning rate of 2500, 3000, and 4000 rpm, respectively. For the same spinning rates, the film thickness are 261 +/- 1, 229 +/- 1, and 204 +/- 1 nm. Optical band gaps of the films, which are estimated from the absorption coefficients, have not changed. The optical band gap is independent of the spin speed and for the direct and indirect transitions the band gaps are 3.30 +/- 0.06, and 2.92 +/- 0.05eV, respectively. (C) 2001 Elsevier Science B.V. All rights reserved. [References: 25]
机译:CeO2-TiO2薄膜已经通过旋涂法以2500、3000和4000 rpm的转速通过溶胶-凝胶工艺沉积在玻璃基板上。通过评估约11周内光谱行为的变化,研究了时间对薄膜光学性能的影响。在老化的第一周,薄膜的光学指数显示出可观察到的变化。四周后,变化减小,并且这些参数大约在六周后变得恒定。老化11周后,发现CeO2-TiO2薄膜的折射率为1.91 +/- 0.03、1.98 +/- 0.04和1.10 +/- 0.02,消光系数为2.8 +/- 0.2 x 10 (-3),纺纱速度分别为2500、3000和4000 rpm时为3.3 +/- 0.2 x 10(-3)和3.8 +/- 0.3 x 10(-3)。对于相同的纺丝速度,膜厚度为261 +/- 1、229 +/- 1和204 +/- 1 nm。由吸收系数估计的膜的光学带隙没有改变。光学带隙与自旋速度无关,对于直接和间接跃迁,带隙分别为3.30 +/- 0.06和2.92 +/- 0.05eV。 (C)2001 Elsevier Science B.V.保留所有权利。 [参考:25]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号