This study reported an environmentally benign approach to iron(III) extraction using undiluted Aliquat 336. This technique was then applied for iron(III) removal from coal mining waste (CMW) hydrochloric acid leach liquor to produce high purity aluminum chloride. The extraction behavior, loading capacity, selectivity, and stripping of iron(III) were investigated within synthetic solutions and compared with those obtained from Cyphos IL 101. The results showed that iron(III) can be quantitatively extracted using Aliquat 336 with high efficiency and high selectivity against aluminum(III), calcium(II), magnesium(II) and potassium(I). The maximum loading capacity of iron(III) in Aliquat 336 was 100.7 g L-1, which is higher than that in Cyphos IL 101. Iron can be more effectively stripped from Aliquat 336 rather than Cyphos IL 101 when using 0.5 M H2SO4 as the stripping solution. The regeneration of the IL phase and their reuse in subsequent extractions of iron from CMW leach liquor were further examined. The extraction efficiency of iron(III) decreased after Aliquat 336 and Cyphos IL 101 had been recycled for six and three cycles, respectively. High purity AlCl3 center dot 6H(2)O crystals were prepared under vacuum evaporation from the raffinate after iron removal, where the iron content in the AlCl3 center dot 6H(2)O crystals was less than 0.005%. (C) 2016 Elsevier B.V. All rights reserved.
机译:这项研究报告了使用未经稀释的Aliquat 336提取铁(III)的一种环境友好方法。该技术随后用于从煤矿废水(CMW)盐酸浸提液中去除铁(III)以生产高纯度氯化铝。在合成溶液中研究了铁(III)的萃取行为,负载量,选择性和汽提,并与从Cyphos IL 101中获得的结果进行了比较。结果表明,使用Aliquat 336可以高效,高效地定量萃取铁(III)。对铝(III),钙(II),镁(II)和钾(I)具有高选择性。 Aliquat 336中铁(III)的最大负载量为100.7 g L-1,高于Cyphos IL 101中的铁。当使用0.5 M H2SO4作为Cyphos IL 101时,铁可以更有效地从Aliquat 336中去除而不是Cyphos IL 101。剥离溶液。 IL相的再生及其在随后从CMW浸出液中提取铁的再利用方面得到了进一步研究。 Aliquat 336和Cyphos IL 101分别循环使用六个和三个循环后,铁(III)的提取效率下降。除去铁后,从萃余液中真空蒸发制备高纯度AlCl3中心点6H(2)O晶体,其中AlCl3中心点6H(2)O晶体中的铁含量小于0.005%。 (C)2016 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号