In this paper, some methods to get piezoelectric ceramic materials for high-temperature and high-frequency applications based on modified PbTiO3 piezoelectric ceramics have been introduced. A solid solution system (1 - X) PbTiO3 + XPb(Cd1/3Nb2/3)O-3 has been studied for its piezoelectric properties as the B-position complex substitution of ABO(3) perovskite structure. The system with X = 14 mol% has good piezoelectric properties by adding some suitably modified additives, such as WO3, MnO2 and NiO. The Curie temperature is over 450 degrees C and the dielectric constant, epsilon(s), is about 200 at room temperature. The piezoelectric coupling factor k(t) is 0.45 and the mechanical quality factor Q(m) can be changed from 500 to 2400 according to different situations. The high stability of these materials makes it possible for them to be used in high-temperature and high-frequency situations. (C) 1998 Elsevier Science S.A. All rights reserved. [References: 10]
机译:本文介绍了一些基于改性PbTiO3压电陶瓷的高温,高频应用压电陶瓷材料的制备方法。研究了固溶体系(1-X)PbTiO3 + XPb(Cd1 / 3Nb2 / 3)O-3的压电性质,作为ABO(3)钙钛矿结构的B位置复合物替代。 X = 14 mol%的体系通过添加一些适当改性的添加剂(例如WO3,MnO2和NiO)具有良好的压电性能。居里温度超过450摄氏度,室温下的介电常数ε约为200。压电耦合系数k(t)为0.45,机械品质因数Q(m)可以根据不同情况从500更改为2400。这些材料的高稳定性使其可以在高温和高频情况下使用。 (C)1998 Elsevier Science S.A.保留所有权利。 [参考:10]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号