Annealing softening mechanisms operating in cold worked oxide-bearing steels

机译:在冷加工含氧化物钢中运行的退火软化机制

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Annealing softening mechanisms operating in cold-worked Fe-O steels were studied at 700 at 800 ℃. Primary recrystallization develops only in 0.2%O samples after cold deformation of ε ≥ 70%. In samples containing 0.6%O, static recovery is the only annealing softening process irrespective of cold deformation intensity.
机译:研究了在700℃,800℃下对冷加工Fe-O钢进行退火的软化机理。 ε≥70%的冷变形后,仅在0.2%O的样品中发生初次重结晶。在含0.6%O的样品中,无论冷变形强度如何,静态恢复都是唯一的退火软化过程。