Comparative study of fatigue behaviour in dissimilar Al alloy/steel and Mg alloy/steel friction stir spot welds fabricated by scroll grooved tool without probe

机译:无探针涡旋开槽刀具在异种铝合金/钢和镁合金/钢摩擦搅拌点焊中疲劳行为的比较研究

获取原文
获取原文并翻译 | 示例
           

摘要

Aluminium alloy A6061-T6 or magnesium alloy AZ31 sheet was welded to steel sheet by a friction stir spot welding technique using a scroll grooved tool without a probe. The material flow in the nugget of the Mg/steel weld was less than that in the Al/steel one. The Al/steel weld exhibited higher static tensile-shear strength than the Al/Al weld, while the strengths of Mg/steel and Mg/Mg welds were comparable. Tensile-shear fatigue tests were performed using lap shear specimens of both dissimilar and similar welds. The dissimilar welds exhibited nearly the same fatigue strengths as the similar ones. The effective nugget size in the dissimilar welds was defined as the area where Al or Mg alloy remained on the steel side after static fracture. When the fatigue strengths of dissimilar welds were evaluated based on the effective nugget size, the normalised fatigue strengths of Al/steel and Mg/steel welds were comparable.
机译:使用不带探头的涡旋开槽工具,通过摩擦搅拌点焊技术将铝合金A6061-T6或镁合金AZ31板焊接到钢板上。镁/钢焊缝熔核中的材料流量少于铝/钢熔核中的材料流。 Al /钢焊缝比Al / Al焊缝具有更高的静态拉伸剪切强度,而Mg /钢和Mg / Mg焊缝的强度却相当。使用不同和相似焊缝的搭接剪切试样进行拉伸剪切疲劳试验。异种焊缝的疲劳强度几乎与同类焊缝相同。异种焊缝中的有效熔核尺寸定义为静态断裂后Al或Mg合金保留在钢侧的区域。当根据有效熔核尺寸评估异种焊缝的疲劳强度时,Al /钢和Mg /钢焊缝的归一化疲劳强度具有可比性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号