Corrosion tests of Inconel 600 and Incoloy 825 were performed in supercritical water containing sulfides at 520 A degrees C and 25 MPa. The scales formed on Inconel 600 consisted of a thick outer layer of almost pure Ni3S2 and an inner layer predominantly of Cr-rich spinels with a Ni3S2 network inside. The scales of Incoloy 825 also had a multilayered structure. The outer layer primarily consisted of Ni3S2 and (Ni,Fe)(3)S-4,S- followed by a thicker intermediate mixture layer of chromium-rich oxides, Ni3S2, and (Ni,Fe)(3)S-4, an inner layer of predominantly Cr2O3 and a small amount of Ni3S2 toward the substrate. Incoloy 825 showed slightly better corrosion resistance than Inconel 600 due to its higher Cr content. By means of superimposed isothermal phase diagrams and evaluation for the partial pressures of oxygen and sulfur in the designated atmosphere, the corresponding corrosion mechanisms were discussed, based on the present investigation.
机译:Inconel 600和Incoloy 825的腐蚀试验是在520 A和25 MPa的含硫化物的超临界水中进行的。在Inconel 600上形成的氧化皮由几乎纯净的Ni3S2的厚外层和主要由富含Cr的尖晶石组成的内层组成,内层具有Ni3S2网络。 Incoloy 825的氧化皮也具有多层结构。外层主要由Ni3S2和(Ni,Fe)(3)S-4,S-组成,然后是较厚的富铬氧化物Ni3S2和(Ni,Fe)(3)S-4中间混合物层,一层主要是Cr2O3的内层和少量朝向基材的Ni3S2。由于Incoloy 825的Cr含量较高,因此其耐腐蚀性比Inconel 600略好。通过叠加等温相图并评估指定气氛中氧气和硫的分压,在此基础上讨论了相应的腐蚀机理。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号