Growth and spectroscopic properties of ytterbium-doped lanthanum calcium borate (Yb~(3+):La_(2)CaB_(10)O_(19)) crystal

机译:掺tter硼酸镧钙(Yb〜(3 +):La_(2)CaB_(10)O_(19))晶体的生长和光谱性质

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

A new ytterbium-doped lanthanum calcium borate crystal (Yb~(3+):La_(2)CaB_(10)O_(19), Yb:LCB) has been grown by the flux method. The spectroscopic properties have been investigated and the fundamental spectral parameters for Yb:LCB crystal have been calculated. Yb:LCB crystal has the strongest absorption at 976 nm with a full-width at half-maximum of 14 nm. The absorption and emission cross-sections are 1.16×10~(-20) and 3.51×10~(-20) cm~(2), respectively. The fluorescence lifetime is 0.95 ms. The ground-state energy level splitting is calculated to be 640 cm~(-1). In comparison with other Yb-doped laser crystals, the calculated parameters show that Yb:LCB crystal satisfies the fundamental spectral condition for laser emission.
机译:通过熔剂法生长了一种新的掺-硼酸镧镧晶体(Yb〜(3 +):La_(2)CaB_(10)O_(19),Yb:LCB)。研究了光谱性质,并计算了Yb:LCB晶体的基本光谱参数。 Yb:LCB晶体在976 nm处吸收最强,半峰全宽为14 nm。吸收截面和发射截面分别为1.16×10〜(-20)和3.51×10〜(-20)cm〜(2)。荧光寿命为0.95ms。计算出的基态能级分裂为640 cm〜(-1)。与其他掺Yb的激光晶体相比,计算得出的参数表明Yb:LCB晶体满足激光发射的基本光谱条件。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号