The topicality is shown to improve the processing technology of complex polymetallic raw material containing a considerable amount of toxic impurities of arsenic and lead. Results on pressure leaching the mattes formed after reduction smelting the dusts of OAO Sredneural'skii Copper Smeltery (SUMZ) by solutions of copper sulfate are discussed. These mattes contain a considerable amount of lead and arsenic. According to the data of X-ray phase analysis of matte samples, phases of sulfides (PbS, PbS a <... As2S3, Cu2S, FeS, and (Zn,Fe)S) and arsenides (FeAs2, Cu3As, FeAs, and Cu0.85As0.15), as well as inclusions of metallic copper, are revealed in them. Optimal parameters of matte leaching by copper sulfate solutions are the temperature of 150-180A degrees C, acidity from 5 to 30 g/dm(3), and copper concentration of 14-32 g/dm(3). This process made it possible to extract 85% As into the solution, while copper and lead remained in the cake in this case.
机译:已显示出局部性可改善包含大量砷和铅有毒杂质的复杂多金属原料的加工技术。讨论了用硫酸铜溶液对OAO Sredneural'skii铜冶炼厂(SUMZ)的粉尘进行还原冶炼后压力浸出形成的冰沙的结果。这些亚光包含大量的铅和砷。根据粗面样品的X射线相分析数据,可以发现硫化物(PbS,PbS a <... As2S3,Cu2S,FeS和(Zn,Fe)S)和砷化物(FeAs2,Cu3As,FeAs和其中发现了Cu0.85As0.15)以及金属铜的夹杂物。硫酸铜溶液中亚铜浸出的最佳参数是温度为150-180A摄氏度,酸度为5至30 g / dm(3)和铜浓度为14-32 g / dm(3)。该过程使得有可能将85%的As提取到溶液中,而在这种情况下,铜和铅保留在滤饼中。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号