首页> 外文期刊>Luminescence: The journal of biological and chemical luminescence >Synthesis and luminescent properties of a novel bluish-white afterglow phosphor, beta-Zn-3(PO4)(2): Hf4+
【24h】

Synthesis and luminescent properties of a novel bluish-white afterglow phosphor, beta-Zn-3(PO4)(2): Hf4+

机译:新型蓝白色余辉荧光粉β-Zn-3(PO4)(2):Hf4 +的合成及发光性能

获取原文
获取原文并翻译 | 示例
           

摘要

A new bluish-white long-lasting phosphorescent material, Hf4+-doped beta-Zn-3(PO4)(2), was prepared by the conventional high-temperature solid-state method. The photoluminescence (PL) spectrum reveals that it exhibits a strong blue emission band centred at 470 nm, with asymmetry on the long wavelength side; this material emits bluish-white light and shows strong afterglow phosphorescence after it is excited with a 254 nm UV lamp. The phosphorescence lasts nearly 40 min in the light perception of the dark-adapted human eye (0.32 mcd/m(2)). The possible phosphorescence mechanism is also analysed. Copyright (c) 2008 John Wiley & Sons, Ltd.
机译:通过常规的高温固态方法制备了一种新型的蓝白色持久磷光材料,即Hf4 +掺杂的β-Zn-3(PO4)(2)。光致发光(PL)光谱显示它显示出一个强的蓝色发射带,中心在470 nm,长波长侧不对称。该材料发出蓝白色光,并在254 nm紫外灯激发后显示出强烈的余辉磷光。在适应深色的人眼(0.32 mcd / m(2))的光感知下,磷光持续近40分钟。还分析了可能的磷光机理。版权所有(c)2008 John Wiley&Sons,Ltd.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号