Synergistic Inhibition of Enamel Demineralization by Peptide 8DSS and Fluoride

机译:肽8DSS和氟化物协同抑制牙釉质脱矿质

获取原文
获取原文并翻译 | 示例
       

摘要

The biomimetic peptide 8DSS has shown beneficial effects in promoting remineralization of demineralized enamel in vitro. Here we examined the ability of 8DSS alone and in combination with fluoride to inhibit enamel demineralization during pH-cycling mimicking intraoral conditions. Enamel blocks were subjected to 9 days of pH-cycling in the presence of 1,000 ppm NaF (positive control), distilled-deionized water (DDW; negative control), 25 mu M 8DSS alone, 25 mu M 8DSS with 500 ppm NaF (8DSS-FL) or 25 mu M 8DSS with 1,000 ppm NaF (8DSS-FH) twice daily for 1 min each time. The blocks were analyzed in terms of surface microhardness (SMH), fluoride uptake and mineral content. The 8DSS-treated blocks showed significantly lower mineral loss, shallower lesions and higher SMH than the DDW-treated blocks. No significant differences were observed between the blocks treated with 8DSS alone or fluoride alone. The blocks treated with 8DSS alone or DDW showed similar amounts of fluoride uptake, which was the lowest of all the treatment groups. The blocks treated with 8DSS-FL or 8DSS-FH did not differ significantly, and both groups showed significantly greater SMH and fluoride uptake as well as significantly lower mineral loss and shallower lesions than the NaF-treated blocks. Mineral content was significantly higher in the 8DSS-treated blocks than in the DDW-treated blocks from the surface layer (10 mu m) to the lesion depth (110 mu m), and it was significantly higher in the blocks treated with 8DSS-FL or 8DSS-FH than in the NaF-treated blocks from 10 to 90 mu m. These findings illustrate the potential of 8DSS for inhibiting enamel demineralization and for enhancing the anticaries effect of NaF. (C) 2016 S. Karger AG, Basel
机译:仿生肽8DSS在体外促进脱矿质牙釉质的再矿化方面显示出有益作用。在这里,我们研究了8DSS单独和与氟化物联合使用在抑制口内条件的pH循环过程中抑制牙釉质脱矿质的能力。在1,000 ppm NaF(阳性对照),蒸馏去离子水(DDW;阴性对照),单独25μM8DSS,25μM8DSS和500 ppm NaF(8DSS)存在下,对搪瓷块进行9天的pH循环-FL)或含1000 ppm NaF的25μM8DSS(8DSS-FH)每天两次,每次1分钟。根据表面显微硬度(SMH),氟化物吸收量和矿物质含量对块进行了分析。与DDW处理的区块相比,经8DSS处理的区块显示出明显更低的矿物质流失,更浅的病变和更高的SMH。单独使用8DSS或单独使用氟化物处理的嵌段之间未观察到显着差异。单独用8DSS或DDW处理的块显示出相似的氟化物吸收量,这是所有治疗组中最低的。用8DSS-FL或8DSS-FH处理的阻滞没有显着差异,并且两组均显示出比NaF处理的阻滞显着更大的SMH和氟化物吸收以及显着更低的矿物质损失和更浅的病变。从表层(10微米)到病变深度(110微米),在8DSS处理的区块中矿物质含量显着高于DDW处理的区块,而在8DSS-FL处理的区块中矿物质含量显着更高或8DSS-FH比NaF处理的块在10至90μm之间。这些发现说明了8DSS抑制牙釉质脱矿质和增强NaF防龋效果的潜力。 (C)2016 S.Karger AG,巴塞尔

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号