Preparation and characterization of Pd loaded Sr-deficient K2NiF4-type (La, Sr)(2)MnO4 catalysts for NO-CO reaction

机译:Pd负载型Sr不足的K2NiF4型(La,Sr)(2)MnO4催化剂的制备及表征

获取原文
获取原文并翻译 | 示例

摘要

Pdloaded K2NiF4-type perovskite oxides, Pd/La0.2Sr1.8-xMnO(4) were prepared by liquid-phase adsorption process, and their structural and catalytic properties were investigated. Pd deposition was carried out by mixing La0.2Sr1.8MnO4 with Pd(NO3)(2) in aqueous solution, followed by filtration, drying, and calcination at 800 degrees C. During the Pd deposition process, 5% of Sr in La0.2Sr1.8MnO4 oxides was dissolved into the aqueous phase, whereas the perovskite structure retained. The content of Pd loaded on La0.2Sr1.8MnO4 was 0.24 wt%. X-ray absorption spectroscopy studies showed that highly dispersed PdO nanoparticles were supported on Pd/La0.2Sr1.8MnO4 prepared by the liquid-phase adsorption process, whereas aggregated PdO particles were formed on Pd/La0.2Sr1.8MnO4 prepared by an impregnation method. The Pd/La0.2Sr1.8MnO4 catalyst prepared by the liquid-phase adsorption process exhibited higher catalyticactivity for NO-CO reaction than the 0.24 wt% Pd/La0.2Sr1.8MnO4 catalyst prepared by the impregnation method. (C) 2014 Elsevier B.V. All rights reserved.
机译:采用液相吸附法制备了Pd负载的K2NiF4型钙钛矿氧化物Pd / La0.2Sr1.8-xMnO(4),并对其结构和催化性能进行了研究。通过将La0.2Sr1.8MnO4与Pd(NO3)(2)在水溶液中混合,然后在800摄氏度下过滤,干燥和煅烧,进行Pd沉积。在Pd沉积过程中,La0中的Sr含量为5%。 2Sr1.8MnO4氧化物溶解在水相中,而钙钛矿结构得以保留。负载在La0.2Sr1.8MnO4上的Pd含量为0.24重量%。 X射线吸收光谱研究表明,液相分散法制备的Pd / La0.2Sr1.8MnO4上负载有高度分散的PdO纳米颗粒,而浸渍法制备的Pd / La0.2Sr1.8MnO4上形成了聚集的PdO颗粒。 。通过液相吸附法制备的Pd / La0.2Sr1.8MnO4催化剂对NO-CO反应的催化活性高于通过浸渍法制备的Pd / La0.2Sr1.8MnO4催化剂。 (C)2014 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号