It is shown that, unlike their crystalline concentrates, the saturated solutions of mineral fertilizers (ammonium sulfate and nitrophoska) cause intense local corrosion damages to 20 steel and St.3 steel. In this case, the corrosion rate attains 0.29-0.33 mm/yr and is 2.2-2.5 times higher than in distilled water. These steels corrode most rapidly during the first day and then the corrosion rate in the nitrophoska solution decreases and becomes comparable with the corrosion rate in distilled water. The steady-state potentials of both steels are most negative in the solution of ammonium sulfate, whereas the corrosion currents are maximum in the nitrophoska solution. The difference between the Tafel constants b_c of (he cathodic reactions for both steels in the investigated media is insignificant and the lowest constant b_a is observed in the nitrophoska solution, which corresponds to the lowest polarization of the anodic reaction.
机译:结果表明,与它们的结晶浓缩物不同,矿物肥料的饱和溶液(硫酸铵和硝磷)对20钢和St.3钢造成强烈的局部腐蚀破坏。在这种情况下,腐蚀速率达到0.29-0.33 mm / yr,比蒸馏水高2.2-2.5倍。这些钢在第一天腐蚀最快,然后在硝基磷溶液中的腐蚀速率下降,并且变得与蒸馏水的腐蚀速率相当。两种钢的稳态电势在硫酸铵溶液中最负,而腐蚀电流在硝基磷溶液中最大。 (在研究的介质中两种钢的阴极反应的塔菲常数b_c之间的差异均不显着,在硝基磷溶液中观察到的最低常数b_a对应于阳极反应的最低极化)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号