Rod-shaped polyaniline (PANI)-barium ferrite nanocomposite was synthesized by in situ polymerization of aniline in the presence of BaFe12O19 nanoparticles with diameters of 60-80 nm. The structure, morphology and properties of the nanocomposite were measured using powder x-ray diffraction, Fourier transform infrared spectroscopy, scanning electron microscopy, transmission electron microscopy and vibrating sample magnetometry. Different ferrite/PANI ratios were selected in order to study magnetic and conductive properties. The results indicated that there were some interactions between PANI chains and ferrite particles. The saturation magnetization and the coercivity varied with the ferrite content. The conductivity at room temperature decreased from 43.35 to 6.9 x 10(-2) S cm(-1) when the ferrite content changed from 0 to 50 wt%. The composite has excellent electromagnetic parameters which indicates potential application in high performance adsorbing materials in broadband and high frequency ranges. The polymerization mechanism and interactions in the nanocomposites were also studied.
机译:棒状聚苯胺(PANI)-钡铁氧体纳米复合材料是通过在直径为60-80 nm的BaFe12O19纳米粒子存在下通过苯胺原位聚合而合成的。使用粉末X射线衍射,傅立叶变换红外光谱,扫描电子显微镜,透射电子显微镜和振动样品磁法测量纳米复合材料的结构,形态和性能。选择不同的铁氧体/ PANI比值以研究磁性和导电性。结果表明,PANI链与铁氧体颗粒之间存在一些相互作用。饱和磁化强度和矫顽力随铁素体含量而变化。当铁氧体含量从0到50 wt%改变时,室温下的电导率从43.35降低到6.9 x 10(-2)S cm(-1)。该复合材料具有出色的电磁参数,这表明它可能在宽带和高频范围内的高性能吸附材料中得到应用。还研究了纳米复合材料中的聚合机理和相互作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号