Nanofillers are added to dental adhesives to improve mechanical properties of the hybrid layer. Ethanol or water added to the demineralized dentin to improve adhesive infiltration may produce filler aggregation. OBJECTIVE: To assess the effect of 5 vol% water or ethanol addition on nanoparticles distribution in dental adhesives. METHODS: Six available commercial adhesives systems were selected: Clearfil SE Bond (CSE), Clearfil Protect Bond (CPB), FL-Bond (FLB), Clearfil S3 (CS3), Bond Force (BF), One Up Bond F plus (OUB), and an experimental adhesive system without filler (EXP). Polymer films were obtained by adding 0 (control) or 5 vol% water or ethanol into the bonding resins. Preparations were light-cured (40 s). Three specimens were analyzed for each mixture. Three phases and 3D images were taken from each specimen by means of an atomic force microscope in taping mode (TM/AFM). Cluster sizes and surface nanoroughness were assessed. RESULTS: Control specimens from CSE, FLB, OUB, and BF presented clusters. The addition of solvents lead to particles aggregation in tested bonding resins. Ethanol addition produced more aggregates, particularly in adhesives containing fluoraluminosilicate as fillers. CONCLUSIONS: Nanofillers aggregation occurred in all adhesive systems in presence of additional solvents. In general, aggregate sizes were higher after the addition of ethanol. Formed clusters size values are always above the dimensions of the spaces existing between the demineralized collagen fibers.
机译:将纳米填料添加到牙科粘合剂中以改善杂化层的机械性能。向脱矿质牙本质中添加乙醇或水以改善粘合剂渗透可能会产生填料聚集。目的:评估添加5体积%的水或乙醇对牙科用胶粘剂中纳米颗粒分布的影响。方法:选择了六种可用的商业胶粘剂系统:Clearfil SE胶粘剂(CSE),Clearfil保护胶粘剂(CPB),FL-Bond(FLB),Clearfil S3(CS3),粘结力(BF),单向粘结F plus(OUB )和不含填料的实验性粘合剂体系(EXP)。通过将0(对照)或5%(体积)的水或乙醇添加到粘合树脂中来获得聚合物薄膜。将制剂光固化(40s)。对每种混合物分析了三个样品。借助于原子力显微镜以包带模式(TM / AFM)从每个样品中获取了三相和3D图像。评估团簇尺寸和表面纳米粗糙度。结果:CSE,FLB,OUB和BF的对照标本呈簇状。添加溶剂会导致颗粒在测试树脂中聚集。乙醇的添加产生更多的聚集体,特别是在含有氟铝硅酸盐作为填料的粘合剂中。结论:在存在附加溶剂的情况下,所有粘合剂体系中均发生纳米填料聚集。通常,加入乙醇后,骨料的粒径更大。形成的簇的尺寸值总是高于脱矿的胶原纤维之间存在的空间的尺寸。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号