Hard-template preparation of Au/CeO2 mesostructured catalysts and their activity for the selective oxidation of 5-hydroxymethylfurfural to 2,5-furandicarboxylic acid

机译:Au / CeO2介孔结构催化剂的硬模板制备及其对5-羟甲基糠醛选择性氧化为2,5-呋喃二甲酸的活性

获取原文
获取原文并翻译 | 示例
           

摘要

Ordered mesoporous CeO2 has been prepared via a hard-template method using SBA-15 as a structure directing agent. Leaching with NaOH and thermal treatment at 500 degrees C enabled the removal of the inorganic template, thus resulting in the formation of long-range ordered CeO2. Nevertheless, small amounts of silica were present in the final oxides. The resulting CeO2 samples were used as supports for Au nanoparticles and the prepared catalysts were tested in the selective oxidation of 5-hydroxymethylfurfural (HMF) to 2,5-furandicarboxylic acid (FDCA). Fine tuning of the silica template removal process was necessary to prepare active materials, by maximizing the close contact between the metal and the support, and thus confirming the important role of ceria defects in 5-hydroxymethylfurfural oxidation to 2,5-furandicarboxylic acid. (C) 2016 Elsevier Inc. All rights reserved.
机译:已通过硬模板法使用SBA-15作为结构导向剂制备了有序的介孔CeO2。用NaOH浸出并在500摄氏度下进行热处理可以除去无机模板,从而导致形成长程有序CeO2。尽管如此,最终的氧化物中仍存在少量的二氧化硅。将所得的CeO2样品用作Au纳米颗粒的载体,并测试了制备的催化剂在5-羟甲基糠醛(HMF)选择性氧化为2,5-呋喃二甲酸(FDCA)中的能力。通过最大化金属与载体之间的紧密接触,必须对二氧化硅模板的去除过程进行微调,以制备活性材料,从而确认二氧化铈缺陷在5-羟甲基糠醛氧化成2,5-呋喃二甲酸中的重要作用。 (C)2016 Elsevier Inc.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号