Precipitate hardening through coherent particles is an important strengthening mechanism in Ni-based IN718 superalloy. The change of coherency state, e.g., loss of coherency, can affect the precipitation kinetics and the efficacy of precipitate hardening. In this work, we predict the critical size of -Ni3Nb precipitates in IN718 to trigger coherency loss using the phase-field approach with available materials parameters from first-principles calculations and from the literature. The predicted critical size lies within the range of experimentally reported values. The effect of coherency loss on precipitate morphology and kinetics, as well as the aging time to reach this critical size during heat treatment, is also predicted and discussed. These predictions provide guidance in controlling the size of precipitates and optimizing the strength of IN718 alloys.
机译:通过相干粒子进行的沉淀硬化是镍基IN718高温合金的重要强化机制。相干状态的变化,例如相干性的丧失,会影响沉淀动力学和沉淀硬化的功效。在这项工作中,我们使用相场方法以及第一原理计算和文献中提供的可用材料参数,预测了IN718中-Ni3Nb沉淀的临界尺寸,以触发相干损失。预测的临界尺寸在实验报告值的范围内。还预测并讨论了相干损失对沉淀物形态和动力学的影响,以及在热处理过程中达到该临界尺寸的老化时间。这些预测为控制沉淀物尺寸和优化IN718合金强度提供了指导。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号