Zinc oxide (ZnO) and silver doped zinc oxide (ZnO:Ag) nanoparticles were prepared using nitrates of zinc and silver as oxidizers and ethylene diaminetetraacetic acid (EDTA) as a fuel via low-temperature combustion synthesis (LCS) at 500 ℃. X-ray diffraction (XRD) pattern indicates the presence of silver in the hexagonal wurtzite structure of ZnO. Fourier transform infrared (FTIR) spectrum indicates the presence of Ag-Zn-O stretching vibration at 510 cm~(-1). Transmission electron microscopy (TEM) images shows that the average particle size of ZnO and ZnO:Ag nanoparticles were found to be 58 nm and 52 nm, respectively. X-ray photoelectron spectroscopy (XPS) data clearly indicates the presence of Ag in ZnO crystal lattice. The above characterization techniques indicate that the incorporation of silver affects the structural and optical properties of ZnO nanoparticles. ZnO:Ag nanoparticles exhibited 3% higher photocatalytic efficiency than pure ZnO nanoparticles. ZnO:Ag nanoparticles show better photocatalytic activity for the degradation of trypan blue (TrB) compared to undoped ZnO nanoparticles.
机译:以锌和银的硝酸盐为氧化剂,乙二胺四乙酸(EDTA)为燃料,通过低温燃烧合成(LCS)在500℃下制备了氧化锌(ZnO)和银掺杂的氧化锌(ZnO:Ag)纳米颗粒。 X射线衍射(XRD)图案表明ZnO的六方纤锌矿结构中存在银。傅立叶红外光谱(FTIR)表明在510 cm〜(-1)处存在Ag-Zn-O拉伸振动。透射电子显微镜(TEM)图像显示,发现ZnO和ZnO:Ag纳米颗粒的平均粒径分别为58 nm和52 nm。 X射线光电子能谱(XPS)数据清楚地表明ZnO晶格中存在Ag。上述表征技术表明,银的掺入影响ZnO纳米颗粒的结构和光学性质。 ZnO:Ag纳米粒子的光催化效率比纯ZnO纳米粒子高3%。与未掺杂的ZnO纳米粒子相比,ZnO:Ag纳米粒子对锥虫蓝(TrB)的降解表现出更好的光催化活性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号