Preparation of Ti Ternary Alloys by Addition of Si to Ti-Mo Alloy Scraps for Carbonitride Application

机译:将Si加到Ti-Mo合金废料中以制备碳氮化物来制备Ti三元合金

获取原文
获取原文并翻译 | 示例

摘要

In this study, Ti-Mo-Si ternary alloy ingots were prepared by the addition of Si (0.25-2.0 mass%) to Ti-10Mo alloy scraps in order to produce the raw materials for titanium carbonitride composites. To investigate the effects of Si addition, the prepared alloys were subjected to hardness, tensile strength, grain size, and phase analyses. The Si-added alloys showed no major changes in their O, N, and C impurity contents. Their hardness increased remarkably in proportion to an increase in the Si content, from 435 Hv to 601 Hv at 2.0 mass%. The tensile strength increased with Si addition up to a maximum of 1.0 mass%, reaching 883 MPa, but after this peak, it decreased sharply because of the brittleness that arose by the formation of titanium silicide.
机译:在这项研究中,通过向Ti-10Mo合金废料中添加Si(0.25-2.0质量%)来制备Ti-Mo-Si三元合金锭,以生产碳氮化钛复合材料的原料。为了研究添加硅的影响,对制备的合金进行了硬度,抗张强度,晶粒尺寸和相分析。含硅合金的O,N和C杂质含量没有重大变化。它们的硬度与Si含量的增加成比例地显着增加,以2.0质量%从435Hv增加至601Hv。硅添加量最大为1.0质量%时,抗拉强度增加,达到883 MPa,但在此峰值后,由于硅化钛的形成而产生的脆性,抗拉强度急剧下降。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号